Arkema Group ORGALLOY® RS 6635 A Polyamide 6.6 Alloy 35% Glass Fiber reinforced
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: Polyamide Alloy, Rigid grade, Nylon 6.6 based Molding of Engineering PartsInformation provided by Arkema Group
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Automotive classification
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|