Arkema Group VOLTALEF® 300 HD PCTFE
Subcategory: Fluoropolymer; Thermoplastic
Material Notes: VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group
| Available Properties |
- Density
- Apparent Bulk Density
- Particle Size
- Deformation
- Hardness, H358/30
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Compressive Yield Strength
- Compressive Modulus
- Izod Impact, Notched
- Coefficient of Friction
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Arc Resistance
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|