Armstrong A-3/A Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass, etc. Information provided by Ellsworth Adhesives.
| Available Properties |
- Viscosity
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Adhesive Bond Strength
- CTE, linear 20°C
- Glass Temperature
- Processing Temperature
- Pot Life
- Color
- Mix Ratio
|
|
|
|
| Property Data |