Armstrong A-12-T Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Provides the same basic properties as A-12, but in thixotropic, non-sag, easily-brushable paste form. An ideal material for use where adhesive flow during cure cannot be tolerated. A-12-T meets the requirements of Mil. Spec. MIL-A-47074 (MIL) Type II, Class 2. Information provided by Ellsworth Adhesives.
| Available Properties |
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Adhesive Bond Strength
- CTE, linear 20°C
- Glass Temperature
- Processing Temperature
- Pot Life
- Color
- Mix Ratio
|
|
|
|