Armstrong A-34 Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: This white paste material is a fast-curing adhesive with a working life of 20-25 minutes in a 100-gram mass. Mixing ratio is a convenient 1:1. A-34 has excellent wetting properties and is suggested for bonds which will be subjected to high humidity or cryogenic temperatures. It is especially suited for bonding ABS to itself or to other substrates, plus a wide range of metals, other plastics, ceramics, or wood. A-34 meets the requirements of Mil. spec. MMM-A-187B. Information provided by Ellsworth Adhesives.
| Available Properties |
- Viscosity
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Adhesive Bond Strength
- CTE, linear 20°C
- Glass Temperature
- Processing Temperature
- Pot Life
- Color
- Mix Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|