Armstrong A-661 Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: A truly unique, two-component, room temperature curing thixotropic epoxy adhesive system, which exhibits good bond strength at service temperatures up to 400°F. Ideal for applications where resistance to high service temperatures is required, but where a room temperature cure is desirable. Information provided by Ellsworth Adhesives.
| Available Properties |
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Adhesive Bond Strength
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Glass Temperature
- Processing Temperature
- Pot Life
- Color
- Mix Ratio
|
|
|
|