Armstrong A-701 Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond strengths and outstanding chemical resistance. Requires elevate cure schedules. Information provided by Ellsworth Adhesives.
| Available Properties |
- Viscosity
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Adhesive Bond Strength
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Glass Temperature
- Processing Temperature
- Pot Life
- Color
- Mix Ratio
|
|
|
|