Arlon 0.015" (0.381 mm) Cured/Uncured Silicone Belting Material with Fiberglass Substrate (51426R015)

 

Subcategory: Silicone; Thermoset; Polymer

Material Notes:
Cured silicone rubber with a minimum thickness of 0.002 in. (0.05 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.005 in. (0.1 mm); 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.015 in ± 0.002 (0.38 mm ± 0.05). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 569.6 g/m² ± 50.86 (16.8 oz./yd.², ± 1.5). Shelf Life: 6 months from date of manufacture at 23.8°C (75°F). Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours.

Information provided by the manufacturer, Arlon Silicone Technologies Division.

Available Properties
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Yield
  • Dielectric Strength
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。