Asahi Kasei Leona® 1300G Polyamide 66 Resin, Glass Reinforced
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: Applications: Automotive: Radiator Tanks, Fuel Injectors, ABS Sensors, Engine Mounts Electrical and Industrial: Heater Tanks, Office Furniture, Small EnginesInformation provided by Asahi Kasei
| Available Properties |
- Specific Gravity
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|