Arlon 0.025" (0.635 mm) Flexible Heater Silicone with Fiberglass Substrate (19606R025)
Subcategory: Silicone; Thermoset; Polymer
Material Notes: 0.004 in ± 0.0015 (1 mm ± 0.038) Cured silicone rubber/Prime Coated 1523 Fiberglass/ 0.007 in ± 0.0015 (0.2 mm ± 0.038) uncured silicone rubber; 0.003 in. (0.8 mm) polyethylene interleave. The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 918.8 g/m² ± 47.5 (27.1 oz./yd.² ± 1.4). Shelf Life: 6 months from date of manufacture at 21°C (70°F). Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours. Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|