Arlon 0.029" (0.7366 mm) Flexible Heater Silicone with Fiberglass Substrate (55579A028 or R33299A028)
Subcategory: Silicone; Thermoset; Polymer
Material Notes: 0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.029 in + 0.003, -0.000 (0.74 mm + 0.08, -0.00). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Blue. Weight: 983.3 g/m² ± 67.8 (29.0 oz./yd.² ± 2.0). Shelf Life: 6 months from the date of manufacture. Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours. Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- UL RTI, Electrical
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|