Arlon 0.008 in. (2032mm) Unsupported/Uncured Thermabond® - II Silicone
Subcategory: Silicone; Thermoset
Material Notes: 0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001 (0.2 mm ± 0.03). Color: Natural (Tan). Weight: 454.3 g/m² ± 33.9 (13.4 oz./yd.² ± 1.0). Shelf Life: 6 months from date of manufacture at 21°C (70°F). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Thermal Impendence is 0.60°C/W, ±0.06 °C/W. Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- Shear Modulus
- Shear Strength
- Dielectric Strength
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|