Arlon Red Silicone Rubber on a Kodacel Carrier (30570R015)
Subcategory: Silicone; Thermoset
Material Notes: Uncured, unsupported silicone rubber with a thickness of 0.015 in ± 0.001 (0.38 mm ± 0.025) on a Kodacel carrier (0.005 in., 0.13 mm nominal thickness); 0.0015 in. (0.038 mm) polyethylene interleave. The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 508.6 g/m² ± 33.9 (15.0 oz./yd.² ± 1.0). Shelf Life: 6 months . Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours. Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|