Arlon Silicone Hose and Duct Material with Fiberglass Substrate (R31031R025)
Subcategory: Silicone; Thermoset; Polymer
Material Notes: 0.005 in. (0.01 mm) minimum Cured silicone rubber/0.015 in. (0.38 mm) nominal Prime Coated 1564 Fiberglass/ 0.005 in (0.01 mm) minimum uncured silicone rubber; 0.003 in. (0.8 mm) polyethylene interleave; overall thickness 0.025 in. ± 0.002 (0.64 mm ±0.05). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 1085 g/m² ± 67.8 (32.0 oz./yd.² ± 2.0). Shelf Life: 6 months from date of manufacture at 23.8°C (75°F). Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours. Applications: Hose and duct material. Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|