Arlon Naturally Translucent Silicone Rubber (10502N085)
Subcategory: Silicone; Thermoset
Material Notes: Unsupported fully cured silicone rubber with a thickness of 0.085 in. ±0.0085 (2.2 mm ±0.22 ); 0.003 in. (0.8 mm) polyethylene interleave. Color: Naturally translucent. Weight: 2479 g/m² ± 248 (73.1 oz./yd.² ± 7.3). Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- Tear Strength
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|