Arlon Red Silicone Press Pad with sandwiched Fiberglass Substrate (55393R062)
Subcategory: Silicone; Thermoset; Polymer
Material Notes: Cured silicone rubber with a minimum thickness of 0.027 in. (0.69 mm)/0.018 in. (0.46 mm) Prime Coated 162 Fiberglass/Cured silicone rubber with a minimum thickness of 0.017 in. (0.43 mm); 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.062 in ±0.005 (1.6 mm ± 0.1). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 2299 g/m² ± 187 (67.8 oz./yd.² ± 5.5). Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|