Arlon 0.020" (0.508 mm) Layer-on-Layer Silicone Traction Motor Insulation (P29609R020)
Subcategory: Silicone; Thermoset
Material Notes: 0.010 in. (0.25 mm) minimum uncured silicone on 0.002 in. (0.5 mm) minimum cured silicone on 0.008 in. (0.2 mm) nominal Prime Coated 7628 Fiberglass; 0.0015 in. (0.038 mm) polyethylene interleave; overall thickness 0.020 in ± 0.001 (0.51 mm ± 0.03). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 627.3 g/m² ± 67.8 (18.5 oz./yd.² ± 2.0). Shelf Life: 6 months from date of manufacture at 23.8°C (75°F). Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours. Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|