Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502N060)
Subcategory: Silicone; Thermoset
Material Notes: Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15 ); 0.003 in. (0.8 mm) polyethylene interleave. Color: Translucent. Weight: 2339 g/m² ± 234 (69.0 oz./yd.² ± 6.9). Applications: Composite vacuum bagging materials. Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- 100% Modulus
- Tear Strength
- Compression Set
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|