Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502R060)
Subcategory: Silicone; Thermoset
Material Notes: Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15); 0.003 in. (0.8 mm) polyethylene interleave. The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 2339 g/m² ± 234 (69.0 oz./yd.² ± 6.9). Applications: Composite vacuum bagging materials. Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- 100% Modulus
- Tear Strength
- Compression Set
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|