Arlon Thermavac® 0.085" (2.159 mm) Uncured Silicone Vacuum Bagging (10842S085)
Subcategory: Silicone; Thermoset
Material Notes: Unsupported fully cured silicone rubber with a thickness of 0.085 in. ±0.0085 (2.2 mm ±0.22 ); 0.003 in. (0.8 mm) polyethylene interleave. Color: Saddle brown. Weight: 2424 g/m² ± 224 (71.5 oz./yd.² ± 7.2). Applications: Composite vacuum bagging materials. Information provided by the manufacturer, Arlon Silicone Technologies Division.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Yield
- Tear Strength
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|