ComAlloy Lubrilon® 635 Nylon 6/6, Carbon Fiber/PTFE Filled, Proprietary Lubricant Package
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Polyamide 6/6; Polyamide 66; Nylon 66; ComAlloy International Company, subsidiary of A. Shulman Inc.
Material Notes: Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Unnotched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|