A. Schulman, Inc. INVISIONTMVX-5060UI, Soft Touch Polyolefin Thermoplastic
Subcategory: Polyolefin; Thermoplastic; Olefinic TPE
Material Notes: Description Invision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability .
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tear Strength
- Colorfastness/Weatherability
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|