A. Schulman, Inc. INVISION™ VX-7060UE, Soft Touch Polyolefin Thermoplastic
Subcategory: Polyolefin; Thermoplastic
Material Notes: Description Invision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low temperature toughness. Application Invision™ VX-6060UE is targeted for automotive extrusion appearance applications. Information provided by A. Schulman.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Colorfastness/Weatherability
|
|
|
|