A. Schulman, Inc. POLYAXIS® CP 812, Stabilized Compounded Rotational Molding Resin
Subcategory: Thermoplastic
Material Notes: Description Polyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from unpigmented resins. Density and ESCR tests were performed on compression molded samples.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- ESCR 100% Igepal®
- Melt Index of Compound
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- UV Stabilization
|
|
|
|
| Property Data |