A. Schulman, Inc. POLYAXIS® CP 813-31, General-Purpose Polyethylene
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: Description Polyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR tests were performed on compression molded samples.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- ESCR 100% Igepal®
- Melt Index of Compound
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- UV Stabilization
|
|
|
|