A. Schulman, Inc. POLYAXIS® PD 2000, Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description Polyaxis PD 2000 is a polypropylene specifically designed from rotational molding. NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR tests were performed on compression molded samples.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- ESCR 100% Igepal®
- Melt Index of Compound
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|