A. Schulman, Inc. POLYAXIS® PD 8020, Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description Polyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR. NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR tests were performed on compression molded samples. Application Polyaxis® PD 8020 is typically used in small chemical tanks and special applications. Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- ESCR 100% Igepal®
- Melt Index of Compound
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|