A. Schulman, Inc. Polyethylene CP 763-01, Extruded, Blow Molding and Injection Molding Grade Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: Description CP 763-01 is an extruded, blow molding, and injection molding grade of low density polyethylene having good processability and heat sealability. Application CP 763-01 meets the specifications contained in FDA Regulation 177.1520 for food contact applications. Information provided by A. Schulman.