A. Schulman, Inc. Polyethylene LP 477-01, High-Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Description LP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and pharmaceutical packages.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- ESCR 100% Igepal®
- Melt Index of Compound
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Brittleness Temperature
|
|
|
|
| Property Data |