A. Schulman, Inc. Polyethylene LP 552-01, Injection Molding, Extrusion Grade Compound
Subcategory: Polyethylene; Thermoplastic
Material Notes: Description LP 522-01 is an injection molding and/or extrusion grade compound Application LP 552-01 meets FDA Regulation CFT 177.1520(c)3.1. Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
|
|
|
|