A. Schulman, Inc. POLYFLAM™ RPP 1058, General Purpose Homopolymer Polypropylene (30% Fiberglass)
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description Polyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- Flammability, UL94
|
|
|
|