A. Schulman, Inc. POLYFORT™ FPP 1068-32 Black, 40% Mineral Filled Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description Polyfort® FPP 1068-32 Black is a 40% mineral filled polypropylene designed for use when improved heat resistance, dimensional stability and high stiffness is needed. Application Applications of FPP 1068-32 include electrical connections, ducts, impeller and housings. Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|