A. Schulman, Inc. POLYFORT™ FPP 1512E, Talc Filled, High Impact Copolymer Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description Polyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. Application Polyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|