A. Schulman, Inc. POLYFORT™ FPP 2388, Glass Reinforced Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description Polyfort® FPP 2388 is a 5% glass reinforced polypropylene.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Unnotched
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |