A. Schulman, Inc. POLYFORT™ FXP 6630, Nylon 6.6 Polypropylene Alloy
Subcategory: Nylon; Polypropylene; Thermoplastic; Nylon 66; Polymer
Material Notes: Description Polyfort® FXP 6630 is a nylon 6.6 / polypropylene alloy with 30% wollastonite.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|