A. Schulman, Inc. Polypropylene PP 1227E-01, High-Impact Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description Polypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Unnotched
- Gardner Impact
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|