A. Schulman, Inc. Polypropylene PP 1817-01, Utility Grade Random Co-Polymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description Polypropylene PP 1817-01 is a utility grade random co-polymer which can be used for general purpose injection molding, extrusion, or blow molding applications. It does not have a gel specification and should therefore, not be used for clear thing wall extrusions where gel may be critical.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|