A. Schulman, Inc. Polypropylene PP 2268-01, High Flow, Impact Copolymer Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description Polypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene. Application PP 2173-01 is intended for use in interior trim applications. Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Flexural Modulus
- Gardner Impact
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |