A. Schulman, Inc. Polypropylene PP 3466-01, Homopolymer Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description Polypropylene PP 3466-01 is a homopolymer polypropylene with the addition of antistatic. This product enhances processing with fast cycle times in injection molding. Application PP 3466-01 meets FDA Regulation 21 CFR 177.1520 and is suitable for food packaging applications not exceeding 212°F (100°C). Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Unnotched
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|