A. Schulman, Inc. Polypropylene PP 3486-01, Homopolymer Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description Polypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application. Application This product is for injection molded applications and is in compliance with the FDA requirements of 21 CFR 177.1520 Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
|
|
|
|