A. Schulman, Inc. Polypropylene PP 3491, Homopolymer Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description Polypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Tenacity
- Elongation at Break
- Melt Temperature
|
|
|
|
| Property Data |