A. Schulman, Inc. POLYTROPE™ CB 1010U-330, Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Olefinic TPE
Material Notes: Description Polytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics suitable for molding large automotive parts such as fascias and airdams.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Gardner Impact
- Brittleness Temperature
|
|
|
|