A. Schulman, Inc. POLYTROPE™ TPP 403, Blow Molding Grade Olefinic Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Olefinic TPE
Material Notes: Description Polytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains special heat stabilizers to allow usage in the under-hood environment. TPP 402 is only available in black compounds and is not UV stable.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Gardner Impact
- Tear Strength
- Brittleness Temperature
|
|
|
|