A. Schulman, Inc. POLYTROPE™ TPP 508, Injection Molding Grade Olefinic Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Olefinic TPE
Material Notes: Description Polytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for molding large automotive parts, such as fascias and air dams. TPP 508 is UV stable, paintable and pigmentable.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Gardner Impact
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|