A. Schulman, Inc. POLYTROPE™ TPP 608, Olefinic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Olefinic TPE
Material Notes: Description Polytrope TPP 608 is an olefinic elastomer exhibiting low thermal expansion, low heat sag and high DOI on painted parts. Application TPP 608 is designed specifically for automotive fascias. Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Gardner Impact
- Impact
- CTE, linear 20°C
- Heat Sag
|
|
|
|
| Property Data |