A. Schulman, Inc. SCHULAFLEX® SF 302, Ethylene-Based Butene Plastomer
Subcategory: Thermoplastic
Material Notes: Description Schulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package. NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR tests were performed on compression molded samples. Application SF302 is ideally suited for products requiring a soft feel. Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- ESCR 100% Igepal®
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength @ Yield
- Elongation at Yield
|
|
|
|