A. Schulman, Inc. PAPERMATCH® T-4228-8, Specialty Masterbatch
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic
Material Notes: Description PAPERMATCH® T-4228-8 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. PAPERMATCH® T-4228-8 is a white, medium opacity grade designed to provide a smooth surface finish. PAPERMATCH® T-4228-8 is generally recommended for cast or blown film applications at 50% usage levels in HDPE.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Ash
- Moisture
- Pellet Count
|
|
|
|
| Property Data |