A. Schulman, Inc. POLYBATCH™ Almond 60186U, Concentrate Based in LLDPE
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; LLDPE
Material Notes: Description POLYBATCH® Almond 60186U is an almond color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. POLYBATCH® 60186U is heavy metal free and is typically recommended for use at 4% addition levels. Application This concentrate was designed to provide color and UV stability in polyolefin plastic lumber or injection molding applications. Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Ash
- Moisture (max)
- Pellet Count
|
|
|
|