A. Schulman, Inc. POLYBATCH™ ASP-2000, Permanent Antistatic Product
Subcategory: Additive/Filler for Polymer; Thermoplastic
Material Notes: Description POLYBATCH® ASP-2000 is a permanent antistatic product. This material is designed to provide immediate antistatic performance and last throughout the lifetime of the polyolefin. POLYBATCH® ASP-2000 will not bloom to the surface and will therefore not interfere with printing. POLYBATCH® ASP-2000 performance is maximized when processed at temperatures between 190 to 230°C (375 to 446°F). Application POLYBATCH® ASP-2000 is typically recommended for us in blown film, injection molding, and blow molding applications at 10 to 15% addition levels depending upon application requirements. This product is not recommended for use in cast film applications. Information provided by A. Schulman.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|