A. Schulman, Inc. POLYBATCH™ Bright While LL80250, Concentrate Based In LLDPE
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; LLDPE
Material Notes: Description POLYBATCH® LL80250 is a bright white masterbatch containing 50% titanium dioxide based in LLDPE. This product has been formulate to provide a brighter, cooler, more fresh appearance over standard white color concentrates. POLYBATCH® LL80250 also offers optimal dispersion and excellent letdown mixing. POLYBATCH® LL80250 is typically recommended for use at 2% addition levels in blow molding applications.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Ash
- Moisture (max)
- Pellet Count
|
|
|
|